GUANIDIN NITRAT ASOSIDAGI (FKG2T-4) KOMPOZIT KORROZIYA INGIBITORI SINTEZI, KISLOTALI MUHITDA QO‘LLANILISHI
Maqola haqida umumiy ma'lumotlar
Ushbu maqolada, guanidin nitrat asosida sintezlangan (FKG2K-4) kompozit ingibitorini 1 M HCl eritmasida uglerodli po‘lat konstruksiyalarini korroziyadan himoya qilish tadqiqoti olib borilgan. Bunda, tadqiqot ishida (FKG2K-4) kompozit ingibitorini turli xil konsentratsiya (250 mg/l, 500 mg/l, 750 mg/l va 1 g/l) va haroratlar (298 K va 323 K) da amaliy tajribalar o‘tkazildi. (FKG2K-4) kompozit ingibitorining po‘lat yuzasida adsorbsiyalanish Lengmyur va Tyomkin izotermalari va SEM analizlari bilan o‘rgnildi va tahlil qilindi. (FKG2K-4) kompozit ingibitorining samaradorligi 74.65% dan 92.68% ekanligi gravimetrik metodga asoslanib topildi.
- Ж Н. П. Курс теории корозии и зашиты металов. М. Металлургии, 1976, с. 492
- Акользин А. П. Противокоррозионная зашита стали пленкообразователями. М.: Металлургия, 1989, с. 192
- Брегман Дж. Ингибиторы коррозии. М.: Химия. 1996.
- Робинсон Д. С. Ингибиторы коррозии. М.: Металлургия, 1983, с. 272.
- N. Ochoa, F. Moran, N. Pébère and B. Tribollet, Corros. Sci., 47 (2005)593.
- P. Ocón, A.B. Cristobal, P. Herrasti and E. Fatas, Corros. Sci., 47 (2005)649.
- E.A. Noor, Corros. Sci., 47 (2005) 33.
- A. Frignani, C. Monticelli, F. Zucchi and G. Trabanelli, Mater. Chem. & phys.92 (2005) 403.
- M. Karaku, M. ahin and S. Bilgiç, Mater. Chem.& phys. 92 (2005) 565.
- . T.A. Sanaa, Inhibition action of thiosemicabazone and some of it is ρ-substituted compounds on the corrosion of iron-base metallic glass alloy in 0.5 M H2SO4 at 30 0C, Mater. Res. Bull. 43 (2008) 510.
- T. Poornima, J. Nayak, A.N. Shetty, Corrosion ofaged and annealed 18 Ni 250 grade maraging steel in phosphoric acid medium, Int. J. Electrochem. Sci. 5 (2010) 56.
- E.E. Oguzie, Corrosion inhibition of aluminium in acidic and alkaline media by Sansevieria trifasciata extract, Corros. Sci. 49 (2007) 1527.
- S. Martinez, I. Stern, Thermodynamic characterization of metal dissolution and inhibitor adsorption processes in the low carbon steel/mimosa tannin/sulfuric acid system, Appl. Surf. Sci. 199 (2002) 83.
Beknazarov, H. S., Jalilov, A. T., & Sharipov, B. S. (2022). GUANIDIN NITRAT ASOSIDAGI (FKG2T-4) KOMPOZIT KORROZIYA INGIBITORI SINTEZI, KISLOTALI MUHITDA QO‘LLANILISHI. Academic Research in Educational Sciences, 3(8), 149–159. https://doi.org/
Beknazarov, Hasan, et al. “GUANIDIN NITRAT ASOSIDAGI (FKG2T-4) KOMPOZIT KORROZIYA INGIBITORI SINTEZI, KISLOTALI MUHITDA QO‘LLANILISHI.” Academic Research in Educational Sciences, vol. 8, no. 3, 2022, pp. 149–159, https://doi.org/.
Beknazarov, S., Jalilov, T., and Sharipov, S. 2022. GUANIDIN NITRAT ASOSIDAGI (FKG2T-4) KOMPOZIT KORROZIYA INGIBITORI SINTEZI, KISLOTALI MUHITDA QO‘LLANILISHI. Academic Research in Educational Sciences. 8(3), pp.149–159.